Your complete guide to cross hatch adhesion testing at Kiyo R&D Lab
Will your coating stay put — or peel, flake, and fail in the field? The fastest, most recognised way to grade coating adhesion is the cross hatch test, where a lattice of cuts is scored into the film and rated by how much coating stays bonded. Looking for a dependable cross hatch tester in chennai, tamilnadu? Kiyo R&D Lab performs cross-hatch adhesion testing to ASTM and ISO methods and grades your coating with confidence.
From paints and powder coatings to primers, plating, and industrial films on metal or plastic, our expert team delivers clear adhesion ratings, supporting photos, and audit-ready reports you can rely on.
A cross hatch test grades how well a coating sticks to its substrate. A special cutting tool scores a lattice of parallel cuts at right angles through the film down to the base material; pressure-sensitive tape is applied over the grid and pulled off, and the amount of coating removed is rated against a standard scale. The equipment used — a cross hatch tester in chennai, tamilnadu — uses fixed, evenly spaced blades so the cut spacing is consistent and the result is repeatable.
It’s fast, low-cost, and widely specified — which is why it’s the go-to adhesion check for incoming inspection, production QC, and coating-failure investigations.
As a full-service cross hatch tester in chennai, tamilnadu, we test paints, powder coatings, primers, plating, and industrial films on metal, plastic, and other substrates, choosing the correct cut spacing for your coating thickness.
Classification on the ASTM/ISO scale.
1 mm or 2 mm spacing by film thickness.
Before/after images of the grid.
Metal, plastic, and coated components.
Lot-by-lot adhesion verification.
Cross-cut, X-cut, and pull-off on request.
| ISO Grade | ASTM Grade | Result |
|---|---|---|
| 0 | 5B | Edges smooth, 0% removed — best |
| 1 | 4B | Small flakes at intersections, <5% |
| 2 | 3B | Flaking along edges, 5–15% |
| 3 | 2B | Flaking in strips, 15–35% |
| 4 | 1B | Large flaking, 35–65% |
| 5 | 0B | Removal greater than 65% — worst |
Note the scales run in opposite directions: ISO 0 and ASTM 5B are both the best result.
Our cross hatch tester in chennai, tamilnadu follows globally recognised methods so your reports are accepted by auditors, buyers, and regulators alike.
ASTM ISO
| Standard | What It Covers | Typical Use |
|---|---|---|
| ASTM D3359 Method B | Cross-cut tape adhesion (lattice) | Standard cross hatch grading |
| ISO 2409 | Cross-cut test for coatings | International cross hatch method |
| ASTM D3359 Method A | X-cut tape adhesion | Thick/rough coatings |
| ISO 16276-2 | Cross-cut & pull-off on protective coatings | Heavy-duty coatings |
| ASTM D4541 | Pull-off adhesion strength | Quantitative complement |
Need a broader adhesion picture? Cross hatch pairs naturally with X-cut and pull-off testing — ask us about combining them.
Based in Chennai with branches in Chrompet and Oragadam, Kiyo R&D Lab makes professional coating adhesion testing easy to access for the Chennai–Oragadam industrial corridor, with convenient drop-off and courier-friendly collection.
Looking for a cross hatch tester in chennai, tamilnadu? Our facilities are equipped for cross-cut, X-cut, and pull-off adhesion testing with quick turnaround.
📞 Call 90420 86986 💬 Request a QuoteExplore all our capabilities at www.kiyorndlab.com.
When coating durability, quality, and compliance are on the line, trust a lab that delivers clear answers. As a leading cross hatch tester in chennai, tamilnadu, we combine calibrated tools, recognised methods, and expert grading to give you results you can stand behind.
From a single adhesion check to ongoing production QC, the team at Kiyo R&D Lab is ready to help. Reach out today and turn your sample into a reliable, audit-ready report.